rubber hose used tire reclaimed rubber
Product Details:
| material | used tire |
|---|---|
| elongation rate | 320%-400% |
| Mooney viscosity, | 70-80 |
| stretch strength | 6.5Mpa-11MPa |
| color | black |
| Place of Origin | Fujian, China (Mainland) |
| Brand Name | Aangfu |
Payment & Shipping Terms:
| Payment Terms: | L/C,T/T |
|---|---|
| Supply Ability: | 200 Metric Ton per Week |
Detailed Product Description
rubber hose used tire reclaimed rubberis made of used tires, applicable for making rubber products such as tires, belts, shoe rubber, with a wide range usage and comprehensive capabilities. Though selecting material carefully, exquisite workmanship,the refined tire reclaimed rubber is a good choice for tires and other high-grade rubber products. And the superfine tire reclaimed rubber is made of fine rubber powder above 60 mesh, it is priority for refined rubber products.
1. The Chemical & Physical Property index of High-quality Tire Reclaimed Rubber: GB/T13460-92
Category/Grade Item | Tire Reclaimed Rubber | ||
Excellent | First grade | Qualified | |
Water content, % ≤ | 1.20 | 1.20 | 1.20 |
Ash content,% ≤ | 10.00 | 12.00 | 15.00 |
Extraction of acetone,% ≤ | 20.00 | 25.00 | 28.00 |
Stretch strength, MPa ≥ | 9.50 | 8.00 | 6.00 |
Elongation rate, % ≥ | 390 | 360 | 320 |
Mooney viscosity ≤ | 70 | 75 | 80 |
2. The Chemical & Physical Property index of Refined Tire Reclaimed Rubber: Q/SHKJ001-2008
Item | Index | ||||
Refine | Superfine | ||||
A Grade | B Grade | C grade | A grade | B grade | |
Water content, % ≤ | 1.00 | 1.10 | 1.20 | 1.00 | 1.10 |
Ash content,% ≤ | 8.00 | 10.00 | 12.00 | 10.00 | 10.00 |
Extraction of acetone,% ≤ | 20.00 | 21.00 | 22.00 | 20.00 | 21.00 |
Stretch strength, MPa ≥ | 9.5 | 8.5 | 6.5 | 8.0 | 6.0 |
Elongation rate, % ≥ | 390 | 370 | 330 | 360 | 320 |
Mooney viscosity, ≤ | 75 | 75 | 80 | 75 | 80 |
3. The Chemical & Physical Property index of Environment-friendly Light Smell Reclaimed Rubber: Q/SHKJ004-2008
Item | Index | |||
A grade | B grade | C grade | D grade | |
Heating loss,% ≤ | 1.10 | 1.10 | 1.20 | 1.20 |
Ash content,% ≤ | 10.00 | 11.00 | 12.00 | 12.00 |
Extraction of acetone, ≤ | 19.00 | 19.50 | 20.00 | 20.00 |
Density, g/cm3 ≤ | 1.18 | 1.19 | 1.20 | 1.20 |
Stretch strength, MPa ≥ | 9.5 | 8.0 | 7.0 | 6.5 |
Elongation rate, % ≥ | 390 | 370 | 360 | 320 |
Mooney viscosity ≤ | 75 | 75 | 80 | 80 |
rubber hose used tire reclaimed rubber
Other Products from this Supplier
See more
rubber hose used tire reclaimed rubber, reclaimed rubber, butyl reclaimed rubber products from this supplier.
Products
- rubber powder [2]
- inner tube [12]
- pine tar [16]
- reclaimed rubber [60]
- Others [5]
Company Info
Fujian Huanke Chemical Rubber Group Co., Ltd.
[China (Mainland)]
[Verified Member]
City: Sanming
Province/State: Fujian
Country/Region : China (Mainland)
Business Type:Manufacturer
Online Postings: Products